USA STANDARDS
Fasteners American Standards
Fastener descriptions to American ANSI and other standards giving dimensional detail of specific products.
Links
| STANDARD | DESCRIPTION | THREAD | MATERIAL | 
| A320L7 | L7 Stud Bolt with Nut A320 | UNC | Steel | 
| A320L7 | Stud Bolt | UNC | Stainless-Steel | 
| ASTMA193 | B7 Stud Bolt with Nut A194 2H | UNC | Steel | 
| ASTMA193 | Stud Bolt B8M with Nut A194 8M | UNC | Stainless-Steel | 
| B1.20.3 | Socket Taper Pressure Pipe Plugs | NPTF 3/4 Taper | Alloy Steel | 
| B1.20.3 | Socket Taper Pressure Pipe Plugs | NPTF 3/4 Taper | Stainless-Steel | 
| B1.20.3 | Socket Taper Pressure Pipe Plugs | NPTF 3/4 Taper | Brass | 
| B1.20.3 | Socket Taper Pressure Pipe Plugs | NPTF 7/8 Taper | Alloy Steel | 
| B1.5 | Allthread ACME | Inch | Grade-5.8 | 
| B1.5 | Allthread ACME | Inch | Stainless-Steel-A2 | 
| B1.5 | Round Flange Track Nut ACME | Inch | Steel | 
| B1.5 | Round Track Nut ACME | Inch | Steel | 
| B16.5 | Flange Bolt | UNC | SAE-5(8.8) | 
| B16.5 | Flange Bolt | UNC | SAE-8(10.9) | 
| B18.15 | Lifting Eye Nut Forged Type A | UNC | Steel | 
| B18.151A | Eye Bolt Forged No Shoulder Type A | UNC | Steel | 
| B18.151B | Eye Bolt Forged No Shoulder Type B | UNC | Steel | 
| B18.152A | Lifting Eye Bolt Forged with Shoulder Collar | UNC | Steel | 
| B18.152B | Lifting Eye Bolt Forged with Shoulder Collar | UNC | Steel | 
| B18.16.3M | Nylon Insert Flange Self Locking Nut | UNC | Steel | 
| B18.2.1 | Hexagon Head Bolt | UNC | SAE-5(8.8) | 
| B18.2.1 | Hexagon Head Set Screw | UNC | SAE-5(8.8) | 
| B18.2.1 | External Torx Bolt with Flange | UNC | SAE-5(8.8) | 
| B18.2.1 | Hexagon Head Bolt | UNC | SAE-8(10.9) | 
| B18.2.1 | Hexagon Head Set Screw | UNC | SAE-8(10.9) | 
| B18.2.1 | External Torx Bolt with Flange | UNC | SAE-8(10.9) | 
| B18.2.1 | External Torx Bolt with Flange | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.2.1 | External Torx Bolt with Flange | UNC | Stainless-Steel 18/10-316-A4 | 
| B18.2.1 | Hexagon Head Bolt | UNF | SAE-5(8.8) | 
| B18.2.1 | Hexagon Head Set Screw | UNF | SAE-5(8.8) | 
| B18.2.1 | Hexagon Head Bolt | UNF | SAE-8(10.9) | 
| B18.2.1 | Hexagon Head Set Screw | UNF | SAE-8(10.9) | 
| B18.2.1.1T10 | Internal External Toothed Shakeproof Washer | Inch | Spring-Steel | 
| B18.2.1.1T10 | Internal External Toothed Shakeproof Washer | Inch | Spring-Steel | 
| B18.2.1.1T6 | Internal Toothed Shakeproof Washer | Inch | Spring-Steel | 
| B18.2.1.1T7 | Internal Toothed Heavy Shakeproof Washer | Inch | Spring-Steel | 
| B18.2.1.1T9 | Countersunk External Toothed Shakeproof Washer | Inch | Spring-Steel | 
| B18.2.1.1T10 | Square Head Bolt | UNC | SAE-5(8.8) | 
| B18.2.1.1T10 | Square Head Bolt | UNC | SAE-8(10.9) | 
| B18.2.1.1T10 | Square Head Bolt | UNC | Mild Steel A-A563 | 
| B18.2.1.1T10 | Square Head Bolt | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.2.1.1T10 | Square Head Bolt | UNC | Stainless-Steel 18/10-316-A4 | 
| B18.2.2 | Hexagon Full Nut | UNC | SAE-5(8.8) | 
| B18.2.2 | Hexagon Heavy Lock Nut | UNC | SAE-5(8.8) | 
| B18.2.2 | Hexagon Heavy Nut | UNC | SAE-5(8.8) | 
| B18.2.2 | Hexagon Lock Nut | UNC | SAE-5(8.8) | 
| B18.2.2 | Hexagon Full Nut | UNC | SAE-8(10.9) | 
| B18.2.2 | Hexagon Heavy Lock Nut | UNC | SAE-8(10.9) | 
| B18.2.2 | Hexagon Heavy Nut | UNC | SAE-8(10.9) | 
| B18.2.2 | Hexagon Lock Nut | UNC | SAE-8(10.9) | 
| B18.2.2 | Hexagon Full Nut | UNC | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Heavy Lock Nut | UNC | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Heavy Nut | UNC | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Lock Nut | UNC | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Machine Screw Nut | UNC | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Allthread Coupling Connector 3D | UNC | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Heavy Nut | UNC | Steel-A194-2H | 
| B18.2.2 | Hexagon Allthread Coupling Connector 3D | UNC | Steel-A194-2H | 
| B18.2.2 | Hexagon Heavy Nut | UNC | Steel C-A563 | 
| B18.2.2 | Hexagon Allthread Coupling Connector 3D | UNC | Steel C-A563 | 
| B18.2.2 | Hexagon Allthread Coupling Connector 3D | UNC | Dh-Steel | 
| B18.2.2 | Hexagon Full Nut | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.2.2 | Hexagon Heavy Lock Nut | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.2.2 | Hexagon Heavy Nut | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.2.2 | Hexagon Lock Nut | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.2.2 | Hexagon Allthread Coupling Connector 3D | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.2.2 | Hexagon Full Nut | UNC | Stainless-Steel 18/10-316-A4 | 
| B18.2.2 | Hexagon Heavy Lock Nut | UNC | Stainless-Steel 18/10-316-A4 | 
| B18.2.2 | Hexagon Heavy Nut | UNC | Stainless-Steel 18/10-316-A4 | 
| B18.2.2 | Hexagon Lock Nut | UNC | Stainless-Steel 18/10-316-A4 | 
| B18.2.2 | Hexagon Allthread Coupling Connector 3D | UNC | Brass | 
| B18.2.2 | Hexagon Structural Heavy Full Nut | UNC | Steel | 
| B18.2.2 | Slotted and Castle Hexagon Nut | UNC | Steel | 
| B18.2.2 | Slotted Hexagon Heavy Nut | UNC | Steel | 
| B18.2.2 | Slotted Hexagon Heavy Nut | UNF | Steel | 
| B18.2.2 | Hexagon Full Nut | UNF | SAE-5(8.8) | 
| B18.2.2 | Hexagon Heavy Lock Nut | UNF | SAE-5(8.8) | 
| B18.2.2 | Hexagon Heavy Nut | UNF | SAE-5(8.8) | 
| B18.2.2 | Hexagon Lock Nut | UNF | SAE-5(8.8) | 
| B18.2.2 | Hexagon Full Nut | UNF | SAE-8(10.9) | 
| B18.2.2 | Hexagon Heavy Lock Nut | UNF | SAE-8(10.9) | 
| B18.2.2 | Hexagon Heavy Nut | UNF | SAE-8(10.9) | 
| B18.2.2 | Hexagon Lock Nut | UNF | SAE-8(10.9) | 
| B18.2.2 | Hexagon Full Nut | UNF | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Heavy Lock Nut | UNF | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Heavy Nut | UNF | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Lock Nut | UNF | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Heavy Nut | UNF | Steel-A194-2H | 
| B18.2.2 | Hexagon Heavy Nut | UNF | Steel C-A563 | 
| B18.2.2 | Hexagon Full Nut | UNF | Stainless-Steel 18/8-304-A2 | 
| B18.2.2 | Hexagon Heavy Lock Nut | UNF | Stainless-Steel 18/8-304-A2 | 
| B18.2.2 | Hexagon Heavy Nut | UNF | Stainless-Steel 18/8-304-A2 | 
| B18.2.2 | Hexagon Lock Nut | UNF | Stainless-Steel 18/8-304-A2 | 
| B18.2.2 | Hexagon Full Nut | UNF | Stainless-Steel 18/10-316-A4 | 
| B18.2.2 | Hexagon Heavy Lock Nut | UNF | Stainless-Steel 18/10-316-A4 | 
| B18.2.2 | Hexagon Heavy Nut | UNF | Stainless-Steel 18/10-316-A4 | 
| B18.2.2 | Hexagon Lock Nut | UNF | Stainless-Steel 18/10-316-A4 | 
| B18.2.2 | Hexagon Full Nut | Left HandUNC | SAE-5(8.8) | 
| B18.2.2 | Hexagon Heavy Lock Nut | Left HandUNC | SAE-5(8.8) | 
| B18.2.2 | Hexagon Heavy Nut | Left HandUNC | SAE-5(8.8) | 
| B18.2.2 | Hexagon Lock Nut | Left HandUNC | SAE-5(8.8) | 
| B18.2.2 | Hexagon Full Nut | Left HandUNC | SAE-8(10.9) | 
| B18.2.2 | Hexagon Heavy Lock Nut | Left HandUNC | SAE-8(10.9) | 
| B18.2.2 | Hexagon Heavy Nut | Left HandUNC | SAE-8(10.9) | 
| B18.2.2 | Hexagon Full Nut | Left HandUNC | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Heavy Lock Nut | Left HandUNC | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Heavy Nut | Left HandUNC | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Lock Nut | Left HandUNC | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Full Nut | Left HandUNF | SAE-5(8.8) | 
| B18.2.2 | Hexagon Heavy Lock Nut | Left HandUNF | SAE-5(8.8) | 
| B18.2.2 | Hexagon Heavy Nut | Left HandUNF | SAE-5(8.8) | 
| B18.2.2 | Hexagon Lock Nut | Left HandUNF | SAE-5(8.8) | 
| B18.2.2 | Hexagon Full Nut | Left HandUNF | SAE-8(10.9) | 
| B18.2.2 | Hexagon Heavy Lock Nut | Left HandUNF | SAE-8(10.9) | 
| B18.2.2 | Hexagon Heavy Nut | Left HandUNF | SAE-8(10.9) | 
| B18.2.2 | Hexagon Full Nut | Left HandUNF | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Heavy Lock Nut | Left HandUNF | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Heavy Nut | Left HandUNF | Mild Steel A-A563 | 
| B18.2.2 | Hexagon Lock Nut | Left HandUNF | Mild Steel A-A563 | 
| B18.2.2 | Square Heavy Nut | UNC | Steel | 
| B18.2.2T1 | Square Nut | UNC | Steel | 
| B18.2.5M | 12 Point Flange Head Bolt | Metric Coarse | Grade-8.8 | 
| B18.2.5M | 12 Point Flange Head Bolt | Metric Coarse | Grade-10.9 | 
| B18.2.5M | 12 Point Flange Head Bolt | Metric Coarse | Grade-12.9 | 
| B18.2.5M | 12 Point Flange Head Bolt | Metric Coarse | Stainless-Steel-A2 | 
| B18.2.5M | 12 Point Flange Head Bolt | Metric Coarse | Stainless-Steel-A4 | 
| B18.2.6 | Hexagon Head Twist Off Tension Control Bolt | UNC | Steel-A325 | 
| B18.2.6 | Round Head Twist Off Tension Control Bolt | UNC | Steel-A325 | 
| B18.2.7.1M | 12 Point Spline Bell Flange Head Bolt | Metric Coarse | Grade-8.8 | 
| B18.2.7.1M | 12 Point Spline Bell Flange Head Bolt | Metric Coarse | Grade-10.9 | 
| B18.2.7.1M | 12 Point Spline Bell Flange Head Bolt | Metric Coarse | Grade-12.9 | 
| B18.2.7.1M | 12 Point Spline Bell Flange Head Bolt | Metric Coarse | Stainless-Steel-A2 | 
| B18.2.7.1M | 12 Point Spline Bell Flange Head Bolt | Metric Coarse | Stainless-Steel-A4 | 
| B18.21.1 | Single Coil Square Section Spring Washer | Inch | Spring-Steel | 
| B18.21.1 | Double Coil Rectangular Section Spring Washer | Inch | Spring-Steel | 
| B18.21.1 | External Toothed Heavy Shakeproof Washer | Inch | Spring-Steel | 
| B18.21.1T1 | Single Coil Regular Section Spring Washer | Inch | Spring-Steel | 
| B18.21.1T2 | Washer Spring, Heavy | Inch | Spring-Steel | 
| B18.21.1T3 | Washer Spring, Extra Duty | Inch | Spring-Steel | 
| B18.21.1T4 | Washer Spring, Hi Collar | Inch | Spring-Steel | 
| B18.21.1T8 | External Toothed Shakeproof Washer | Inch | Spring-Steel | 
| B18.22.1 | Narrow Washer Table 2B | Inch | Steel | 
| B18.22.1 | Regular Washer Table 2B | Inch | Steel | 
| B18.22.1 | SAE Narrow Washer Table 1A | Inch | Steel | 
| B18.22.1 | USS Wide Washer Table 1A | Inch | Steel | 
| B18.22.1 | Wide Washer Table 2B | Inch | Steel | 
| B18.22.1 | Narrow Washer Table 2B | Inch | Stainless-Steel 18/8-304-A2 | 
| B18.22.1 | Regular Washer Table 2B | Inch | Stainless-Steel 18/8-304-A2 | 
| B18.22.1 | SAE Narrow Washer Table 1A | Inch | Stainless-Steel 18/8-304-A2 | 
| B18.22.1 | USS Wide Washer Table 1A | Inch | Stainless-Steel 18/8-304-A2 | 
| B18.22.1 | Wide Washer Table 2B | Inch | Stainless-Steel 18/8-304-A2 | 
| B18.22.1 | Thin Washer Table 1B | Inch | Steel | 
| B18.22M | American Flat Washer Narrow | Metric | Steel | 
| B18.22M | American Flat Washer Regular | Metric | Steel | 
| B18.22M | American Flat Washer Wide | Metric | Steel | 
| B18.22M | American Flat Washer Narrow | Metric | Stainless-Steel 18/8-304-A2 | 
| B18.22M | American Flat Washer Regular | Metric | Stainless-Steel 18/8-304-A2 | 
| B18.22M | American Flat Washer Wide | Metric | Stainless-Steel 18/8-304-A2 | 
| B18.3 | Socket Cap Screw 1960 | UNF | Grade-12.9, Rc38/43 | 
| B18.3 | Socket Set Screw Cone Point | UNC | Grade-14.9-45H | 
| B18.3 | Socket Set Screw Cup Point | UNC | Grade-14.9-45H | 
| B18.3 | Socket Set Screw Dog Point | UNC | Grade-14.9-45H | 
| B18.3 | Socket Set Screw Flat Point | UNC | Grade-14.9-45H | 
| B18.3 | Socket Set Screw Full Dog Point | UNC | Grade-14.9-45H | 
| B18.3 | Socket Set Screw Oval Point | UNC | Grade-14.9-45H | 
| B18.3 | Socket Set Screw Tip Brass | UNC | Grade-14.9-45H | 
| B18.3 | Socket Set Screw Tip Nylon | UNC | Grade-14.9-45H | 
| B18.3 | Low Head Socket Cap Screw | UNC | Steel | 
| B18.3 | Socket Button Head Screw | UNC | Grade-12.9 | 
| B18.3 | Socket Countersunk Screw | UNC | Grade-12.9 | 
| B18.3 | Hexagon Socket Shoulder Screw | UNC | Grade-12.9 | 
| B18.3 | Splined Socket Button Head Screw | UNC | Grade-12.9 | 
| B18.3 | Spline Socket Countersunk Screw | UNC | Grade-12.9 | 
| B18.3 | Torx Socket Button Head Screw | UNC | Grade-12.9 | 
| B18.3 | Torx Socket Countersunk Screw | UNC | Grade-12.9 | 
| B18.3 | Socket Cap Screw 1960 | UNC | Grade-12.9, Rc38/43 | 
| B18.3 | Socket Cap Screw 1960 | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.3 | Socket Button Head Screw | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.3 | Socket Countersunk Screw | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.3 | Hexagon Socket Shoulder Screw | UNC | Stainless-Steel | 
| B18.3 | Low Head Socket Cap Screw | UNC | Stainless-Steel 18/10-316-A4 | 
| B18.3 | Socket Cap Screw 1960 | UNC | Brass | 
| B18.3 | Socket Button Head Screw | UNC | Brass | 
| B18.3 | Socket Countersunk Screw | UNC | Brass | 
| B18.3 | Socket Cap Screw 1960 | UNC | Aluminium | 
| B18.3 | Socket Button Head Screw | UNC | Aluminium | 
| B18.3 | Socket Countersunk Screw | UNC | Aluminium | 
| B18.3 | Socket Cap Screw 1960 | UNC | Monel | 
| B18.3 | Socket Button Head Screw | UNC | Monel | 
| B18.3 | Socket Countersunk Screw | UNC | Monel | 
| B18.3 | Socket Cap Screw 1960 | UNC | Nylon-66 | 
| B18.3 | Socket Button Head Screw | UNC | Nylon-66 | 
| B18.3 | Socket Countersunk Screw | UNC | Nylon-66 | 
| B18.3 | Socket Cap Screw 1960 | UNC | Phospher-Bronze | 
| B18.3 | Socket Button Head Screw | UNC | Phospher-Bronze | 
| B18.3 | Socket Countersunk Screw | UNC | Phospher-Bronze | 
| B18.3 | Socket Set Screw Tip Silver | UNC | Steel | 
| B18.3 | Socket Flange Cap Screw | UNC | Steel | 
| B18.3 | Hexagon Keys Long Arm | Inch | Steel | 
| B18.3 | Hexagon Keys Short Arm | Inch | Steel | 
| B18.3 | Hexagon Keys Long Arm | Inch | Alloy Steel | 
| B18.3 | Hexagon Keys Short Arm | Inch | Alloy Steel | 
| B18.3 | Socket Button Head Screw | UNF | Grade-12.9 | 
| B18.3 | Socket Countersunk Screw | UNF | Grade-12.9 | 
| B18.3 | Splined Socket Button Head Screw | UNF | Grade-12.9 | 
| B18.3 | Spline Socket Countersunk Screw | UNF | Grade-12.9 | 
| B18.3 | Torx Socket Button Head Screw | UNF | Grade-12.9 | 
| B18.3 | Torx Socket Countersunk Screw | UNF | Grade-12.9 | 
| B18.3 | Socket Set Screw Cone Point | UNF | Grade-14.9-45H | 
| B18.3 | Socket Set Screw Cup Point | UNF | Grade-14.9-45H | 
| B18.3 | Socket Set Screw Dog Point | UNF | Grade-14.9-45H | 
| B18.3 | Socket Set Screw Flat Point | UNF | Grade-14.9-45H | 
| B18.3 | Socket Set Screw Full Dog Point | UNF | Grade-14.9-45H | 
| B18.3 | Socket Cap Screw 1960 | UNF | Stainless-Steel 18/10-316-A4 | 
| B18.3 | Socket Button Head Screw | UNF | Stainless-Steel 18/10-316-A4 | 
| B18.3 | Socket Countersunk Screw | UNF | Stainless-Steel 18/10-316-A4 | 
| B18.3 | Socket Cap Screw 1960 | UNF | Brass | 
| B18.3 | Socket Button Head Screw | UNF | Brass | 
| B18.3 | Socket Countersunk Screw | UNF | Brass | 
| B18.3 | Socket Cap Screw 1960 | UNF | Aluminium | 
| B18.3 | Socket Button Head Screw | UNF | Aluminium | 
| B18.3 | Socket Countersunk Screw | UNF | Aluminium | 
| B18.3 | Socket Cap Screw 1960 | UNF | Monel | 
| B18.3 | Socket Button Head Screw | UNF | Monel | 
| B18.3 | Socket Countersunk Screw | UNF | Monel | 
| B18.3 | Socket Cap Screw 1960 | UNF | Nylon-66 | 
| B18.3 | Socket Button Head Screw | UNF | Nylon-66 | 
| B18.3 | Socket Countersunk Screw | UNF | Nylon-66 | 
| B18.3 | Socket Cap Screw 1960 | UNF | Phosphor-Bronze | 
| B18.3 | Socket Button Head Screw | UNF | Phosphor-Bronze | 
| B18.3 | Socket Countersunk Screw | UNF | Phosphor-Bronze | 
| B18.3.3M | Hexagon Socket Shoulder Screw f9 | Metric Coarse | Grade-12.9 | 
| B18.3.3M | Hexagon Socket Shoulder Screw f9 | Metric Coarse | Stainless-Steel | 
| B18.31M | Engineers Stud Metal End =1.1/2 D | Metric Coarse | Steel | 
| B18.5 | Rib Neck Carriage Bolt | UNC | SAE-5(8.8) | 
| B18.5 | Cup Square Neck Carriage Bolt | UNC | SAE-5(8.8) | 
| B18.5 | Cup Square Neck Carriage Bolt Full Thread | UNC | SAE-8(10.9) | 
| B18.6.2 | Square Head Set Screw Cone Pt | UNC | Case Hardened Steel | 
| B18.6.2 | Square Head Set Screw Cup Point | UNC | Case Hardened Steel | 
| B18.6.2 | Square Head Set Screw Half Dog Pt | UNC | Case Hardened Steel | 
| B18.6.2 | Square Head Set Screw Flat Pt | UNC | Case Hardened Steel | 
| B18.6.2 | Square Head Set Screw Oval Pt | UNC | Case Hardened Steel | 
| B18.6.2 | Square Head Set Screw Cup Point | UNC | Alloy Steel | 
| B18.6.2 | Square Head Set Screw Cup Point | UNC | Stainless-Steel | 
| B18.6.2 | Slotted Grub (Set) Screw Flat Point | UNC | Grade-14.9-45H | 
| B18.6.2 | Square Head Set Screw Cup Point | UNF | Case Hardened Steel | 
| B18.6.2 | Slotted Grub (Set) Screw Flat Point | UNF | Grade-14.9-45H | 
| B18.6.3 | Phillips Pan Head Screw | UNC | Grade-4.8 | 
| B18.6.3 | Phillips Raised Countersunk Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Phillips Raised Trim Countersunk Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Slotted Cheese Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Phillips Countersunk Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Phillips 100 Deg Countersunk Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Phillips Trim Countersunk Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Slotted 100 Deg Countersunk Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Slotted Countersunk Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Slotted Pan Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Square Machine Screw Nut | UNC | Mild Steel A-A563 | 
| B18.6.3 | Square Machine Screw Nut | UNC | Stainless-Steel-A2 | 
| B18.6.3 | Square Machine Screw Nut | UNC | Brass | 
| B18.6.3 | Slotted 100 Deg Countersunk Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Slotted Raised Countersunk Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Slotted Raised Countersunk Trim Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi Raised Countersunk Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi Raised Countersunk Trim Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Slotted Mushroom Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Phillips Mushroom Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi Countersunk Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi 100 Deg Countersunk Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi Trim Countersunk Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Slotted Binding Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi Binding Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Phillips Binding Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi Raised Cheese Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi Flange Pan Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Hexagon Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Hexagon Head Machine Screw Large Head | UNC | Grade-4.8 | 
| B18.6.3 | Hexagon Head Slotted Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Hexagon Head Pozi Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Hexagon Head Phillips Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Hexagon Large Head Slotted Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Hexagon Large Head Pozi Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Hexagon Large Head Phillips Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Hexagon Washer Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Hexagon Washer Head Slotted Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Hexagon Washer Head Pozi Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Hexagon Washer Head Phillips Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi Mushroom Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi Pan Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi Pan Washer Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi Round Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.3 | Pozi Round Washer Head Machine Screw | UNC | Grade-4.8 | 
| B18.6.4 | Pozi Pan Head Self Tapping Screw AB | Inch | Case Hardened Steel | 
| B18.6.9A | Wing Nut American Type A | UNC | Steel Cold Forged | 
| B18.6.9A | Wing Nut American Type A | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.6.9A | Wing Nut American Type A | UNC | Stainless-Steel 18/10-316-A4 | 
| B18.6.9A | Wing Nut American Type A | UNC | Brass | 
| B18.6.9A | Wing Nut American Type A | UNF | Steel Cold Forged | 
| B18.6.9B1 | Wing Nut Mickey Mouse B1 | UNC | Steel Cold Forged | 
| B18.6.9B1 | Wing Nut Mickey Mouse B1 | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.6.9B1 | Wing Nut Mickey Mouse B1 | UNC | Stainless-Steel 18/10-316-A4 | 
| B18.6.9B1 | Wing Nut Mickey Mouse B1 | UNC | Brass | 
| B18.6.9B2 | Wing Nut Mickey Mouse Tall B2 | UNC | Steel Cold Forged | 
| B18.6.9B2 | Wing Nut Mickey Mouse Tall B2 | UNC | Stainless-Steel 18/8-304-A2 | 
| B18.6.9B2 | Wing Nut Mickey Mouse Tall B2 | UNC | Stainless-Steel 18/10-316-A4 | 
| B18.6.9B2 | Wing Nut Mickey Mouse Tall B2 | UNC | Brass | 
| B18.6.9C1 | Wing Nut American Type C1 Die Cast | UNC | Die Cast Zinc-Alloy | 
| B18.6.9C2 | Wing Nut American Type C2 Die Cast | UNC | Die Cast Zinc-Alloy | 
| B18.6.9C3 | Wing Nut American Type C3 Die Cast | UNC | Die Cast Zinc-Alloy | 
| B18.6.9D1 | Wing Nut American Type D1 Stamped | UNC | Steel | 
| B18.6.9D2 | Wing Nut American Type D2 Stamped | UNC | Steel | 
| B18.6.9D3 | Wing Nut American Type D3 Stamped | UNC | Steel | 
| B18.8.1 | Split Cotter Pin | Inch | Steel | 
| B18.8.2 | Parallel Dowel Pin | Inch | Hardened & Ground Steel | 
| B18.8.2 | Spring Tension Pin Slotted | Inch | Spring-Steel | 
| B18.8.2 | Spring Tension Pin Slotted | Inch | Stainless-Steel | 
| B18.8.2 | Parallel Dowel Pin | Inch | Stainless-Steel | 
| B18.8.2Coil | Coiled Roll Spring Tension Pin Heavy Duty | Inch | Spring-Steel | 
| B18.8.2Coil | Coiled Roll Spring Tension Pin Light Duty | Inch | Spring-Steel | 
| B18.8.2Coil | Coiled Roll Spring Tension Pin Standard | Inch | Spring-Steel | 
| B18.8.2Coil | Coiled Roll Spring Tension Pin Heavy Duty | Inch | Stainless-Steel | 
| B18.8.2Coil | Coiled Roll Spring Tension Pin Light Duty | Inch | Stainless-Steel | 
| B18.8.2Coil | Coiled Roll Spring Tension Pin Standard | Inch | Stainless-Steel | 
| B18.9 | Countersunk Nib Bolt | UNC | SAE-8(10.9) | 
| B18.9 | Domed Countersunk Square Plow Bolt #3 | UNC | SAE-5(8.8) | 
| B18.9 | Domed Countersunk Square Plow Bolt #3 | UNC | SAE-8(10.9) | 
| B18.9 | Countersunk Square Plow Bolt | UNC | SAE-5(8.8) | 
| B18.9 | Countersunk Square Plow Bolt | UNC | SAE-8(10.9) | 
| B18.9 | Countersunk Square Plow Bolt | UNC | Grade-A(4.6) | 
Inch fastener products are still the norm in the USA the change over to metric has been slow and primarily in the light automotive industry or companies that export products containing fasteners bolts nuts washers and screw.