Metric Coarse Sems Self Tapping Screws with Washer Case Hardened Steel ISO10644
Loading...
Zoom

Metric Coarse Sems Self Tapping Screws with Washer Case Hardened Steel ISO10644

SKU: 2298
Details
Details
Metric Coarse Sems Self Tapping Screws with Washer Case Hardened Steel ISO10644
dab maxdsd6900N nom hd6900N nom d2d6900L nomd6900L d2
ST2.20.80002.10001.00005.00001.00007.0000
ST2.91.10002.80001.00007.00001.00009.0000
ST3.51.30003.30001.00008.00001.000011.0000
ST4.21.40004.03001.00009.00001.000012.0000
ST4.81.60004.54001.000010.00001.600015.0000
ST5.51.80005.22001.600012.00001.600015.0000
ST6.31.80005.93001.600014.00001.600018.0000
ST82.10007.76001.600016.00002.000024.0000
ST9.52.10009.43002.000020.00002.500030.0000