Metric Coarse Ht Sems Screws with Conical Washer Grade-10.9 DIN69005
SKU:
2295
Details
Details
Metric Coarse Ht Sems Screws with Conical Washer Grade-10.9 DIN69005
d | a | l2 min | DIN 6908 h | DIN 6908 d2 |
---|
M2.5 | 0.9000 | 4.0000 | 0.7200 | 6.0000 |
M3 | 1.0000 | 4.0000 | 0.8500 | 7.0000 |
M3.5 | 1.2000 | 6.0000 | 1.0600 | 8.0000 |
M4 | 1.4000 | 6.0000 | 1.3000 | 9.0000 |
M5 | 1.6000 | 6.0000 | 1.5500 | 11.0000 |
M6 | 2.0000 | 8.0000 | 2.0000 | 14.0000 |
M8 | 2.5000 | 10.0000 | 2.6000 | 18.0000 |
M10 | 3.0000 | 12.0000 | 3.2000 | 23.0000 |
M12 | 3.5000 | 14.0000 | 3.9500 | 29.0000 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | Grade-10.9 |
---|
Standard Number | DIN69005 |
---|
Second Standard | ISO10644 |
---|
Drive | Various |
---|
Head | Various |
---|
American Generic Brand Term | - |
---|
Diameter | M2.5,M3,M3.5,M2.5,M3,M3.5,M8,M10,M12 |
---|
Length | 12,14,16,18,20,22,24,26,28,30,35,40,45,50 |
---|