Metric Round Head Solid Rivet Stainless-Steel-A2 DIN660


d         d2            k            d3 min  e       
11.80000.60000.950.50
1.22.10000.70001.15 0.60 
1.42.40000.80001.35 0.70 
1.62.80001.00001.55 0.80 
23.50001.20001.871.00
2.54.40001.50002.37 1.25 
35.20001.80002.87 1.50 
3.56.20002.10003.401.75 
47.00002.40003.872.00 
58.80003.00004.82 2.50
610.50003.60005.82 3.00 
712.20004.20006.82 3.50 
814.00004.80007.76 4.00 

 

 

 

din 660