Metric Taper Pin with Threaded End Steel DIN7977
SKU:
2014
Details
Details
Metric Taper Pin with Threaded End Steel DIN7977
d1 | d2 | b | l min | l max |
---|
5 | M5 | 14.0000 | 40.0000 | 50.0000 |
6 | M6 | 18.0000 | 40.0000 | 60.0000 |
8 | M8 | 22.0000 | 50.0000 | 100.0000 |
10 | M10 | 24.0000 | 60.0000 | 120.0000 |
12 | M12 | 27.0000 | 75.0000 | 140.0000 |
14 | M12 | 30.0000 | 85.0000 | 140.0000 |
16 | M16 | 35.0000 | 85.0000 | 160.0000 |
20 | M16 | 35.0000 | 100.0000 | 160.0000 |
25 | M20 | 40.0000 | 100.0000 | 160.0000 |
30 | M24 | 46.0000 | 160.0000 | 280.0000 |
40 | M30 | 58.0000 | 180.0000 | 300.0000 |
50 | M36 | 70.0000 | 200.0000 | 300.0000 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | STEEL |
---|
Standard Number | DIN7977 |
---|
Second Standard | ISO8737 |
---|
Drive | Non |
---|
Head | NON |
---|
American Generic Brand Term | - |
---|
Diameter | M5,M6,M8,M10,M12,M12,M16,M16,M20,M24,M30,M36 |
---|
Length | 40,45,50,70,90,110,140,160,180,200,220,250,280 |
---|