Inch Coiled Roll Spring Tension Pin Standard Stainless-Steel B18.8.2 Coil
SKU:
2051
Details
Details
Inch Coiled Roll Spring Tension Pin Standard Stainless-Steel B18.8.2Coil
| d | d | Max. | Min. | d2 max | a | hole max | hole min |
|---|
| 1/32" | 0.0310 | 0.0350 | 0.0330 | 0.0290 | 0.0240 | 0.0320 | 0.0310 |
| | 0.0390 | 0.0440 | 0.0410 | 0.0370 | 0.0240 | 0.0400 | 0.0390 |
| 3.64" | 0.0470 | 0.0520 | 0.0490 | 0.0450 | 0.0240 | 0.0480 | 0.0470 |
| | 0.0520 | 0.0570 | 0.0540 | 0.0500 | 0.0240 | 0.0530 | 0.0510 |
| 1/16" | 0.0620 | 0.0720 | 0.0670 | 0.0590 | 0.0280 | 0.0650 | 0.0610 |
| 5/64" | 0.0780 | 0.0880 | 0.0830 | 0.0750 | 0.0320 | 0.0810 | 0.0770 |
| 3/32" | 0.0940 | 0.1050 | 0.0990 | 0.0910 | 0.0380 | 0.0970 | 0.0930 |
| 7/64" | 0.1090 | 0.0120 | 0.1140 | 0.1060 | 0.0380 | 0.1120 | 0.1080 |
| 1/8" | 0.1250 | 0.1380 | 0.1310 | 0.1210 | 0.0440 | 0.1290 | 0.1240 |
| 5/32" | 0.1560 | 0.1710 | 0.1630 | 0.1520 | 0.0480 | 0.1600 | 0.1550 |
| 3/16" | 0.1880 | 0.2050 | 0.1960 | 0.1820 | 0.0550 | 0.1920 | 0.1850 |
| 7/32" | 0.2190 | 0.2380 | 0.2280 | 0.2140 | 0.0650 | 0.2240 | 0.2170 |
| 1/4" | 0.2500 | 0.2710 | 0.2600 | 0.2430 | 0.0650 | 0.2560 | 0.2470 |
| 5/16" | 0.3120 | 0.3370 | 0.3240 | 0.3040 | 0.0800 | 0.3180 | 0.3080 |
| 3/8" | 0.3750 | 0.4030 | 0.3880 | 0.3660 | 0.0950 | 0.3830 | 0.3700 |
| 7/16" | 0.4380 | 0.4690 | 0.4530 | 0.4270 | 0.0950 | 0.4460 | 0.4310 |
| 1/2" | 0.5000 | 0.5350 | 0.5160 | 0.4880 | 0.1100 | 0.5100 | 0.4930 |
| 5/8" | 0.6250 | 0.6610 | 0.6420 | 0.6130 | 0.1250 | 0.6350 | 0.6180 |
| 3/4" | 0.7500 | 0.7870 | 0.7680 | 0.7380 | 0.1500 | 0.7600 | 0.7430 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Stainless-Steel |
|---|
| Standard Number | B18.8.2Coil |
|---|
| Second Standard | - |
|---|
| Drive | Non |
|---|
| Head | NON |
|---|
| American Generic Brand Term | SELOK,SPIROL,HEADLAND |
|---|
| Diameter | 1/32",3.64",1/16",5/64",3/32",7/64",1/8",5/32",3/16",7/32",1/4",5/16",3/8",7/16",1/2",5/8",3/4" |
|---|
| Length | 3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4." |
|---|
Reviews