Technical Information
Fastener Specific
Supply Source

Metric Coarse Extractable Parallel Dowel Pin Case hard steel ISO8735B
Loading...
Zoom

Metric Coarse Extractable Parallel Dowel Pin Case hard steel ISO8735B

SKU: 2541
Details
Details

Metric Coarse Extractable Parallel Dowel Pin Case hard steel ISO8735B


d1681012162025304050
d=m6 min0.0040.0060.0060.0070.0070.0080.008   
d=m6 max0.0120.0150.0150.0180.0180.0210.021   
a approx0.801.001.201.602.002.503.004.005.006.30
c2.102.363.003.804.606.006.007.008.0010.00
d2M3M4M6M6M8M10M16M20M20M24
d34.305.306.406.408.4010.5017.0021.0021.0025.00
t16.008.0010.0012.0016.0018.0024.0030.0030.0036.00
t2 min10.0012.0016.0020.0025.0028.0035.0040.0040.0050.00
t31.001.201.201.201.501.502.002.002.502.50

Metric Coarse Extractable Parallel Dowel Pin Case hard steel ISO 8735 B pull

Additional Info