Metric Extractable Taper Pin Steel DIN7978

SKU: 2011
Details
Details
Metric Extractable Taper Pin Steel DIN7978
d1 d2 a approx t1 t2l minl max
6 M40.80006.000010.000016.0000100.0000
8 M51.00008.000012.000024.0000100.0000
10 M61.200010.000016.000028.0000120.0000
12 M81.600012.000020.000036.0000100.0000
16 M102.000016.000025.000050.0000100.0000
20 M122.500018.000027.000050.0000120.0000
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberDIN7978
Second StandardISO8736
DriveNon
HeadNON
American Generic Brand Term-
Diameter M4,M5,M6,M8,M10,M12
Length16,18,20,25,30,35,40,45,50,70,90,110,120