Technical Information
Fastener Specific
Supply Source

Metric Coiled Roll Spring Tension Pin Heavy Duty Stainless-Steel DIN7344
Loading...
Zoom

Metric Coiled Roll Spring Tension Pin Heavy Duty Stainless-Steel DIN7344

SKU: 2018
Details
Details
Metric Coiled Roll Spring Tension Pin Heavy Duty Stainless-Steel DIN7344
Dd1 mimd1 maxd2 maxa minshole minhole maxl minl max
1.51.61001.71001.40000.50000.13001.50001.60004.000024.0000
22.11002.21001.90000.70000.17002.00002.10004.000040.0000
2.52.62002.73002.40000.70000.21002.50002.60005.000045.0000
33.12003.25002.90000.90000.25003.00003.10006.000050.0000
3.53.64003.79003.40001.00000.29003.50003.62006.000050.0000
44.15004.30003.90001.10000.33004.00004.12008.000060.0000
55.15005.35004.85001.30000.42005.00005.120010.000060.0000
66.18006.40005.85001.50000.50006.00006.120012.000075.0000
88.25008.55007.80002.00000.67008.00008.150016.0000120.0000
1010.300010.65009.75002.50000.840010.000010.150020.0000120.0000
1212.300012.750011.70003.00001.000012.000012.200024.0000160.0000
1616.400016.900015.60004.00001.300016.000016.300032.0000200.0000