D | h | d3 | d4 | L |
---|
2.5 | 9—11.2 | 2.2500 | 20.0000 | 42.0000 |
3.2 | 11.3—14 | 2.8000 | 20.0000 | 48.0000 |
4 | 14.1—20 | 3.6000 | 20.0000 | 64.0000 |
5 | 20.1—26 | 4.5000 | 25.0000 | 80.0000 |
6.3 | 26.1—34 | 5.6000 | 25.0000 | 97.0000 |
7 | 34.1—45 | 6.3000 | 30.0000 | 125.0000 |
8 | 45.1—56 | 7.0000 | 30.0000 | 150.0000 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | Spring-Steel |
---|
Standard Number | DIN11024 |
---|
Second Standard | - |
---|
Drive | - |
---|
Head | - |
---|
American Generic Brand Term | R PIN |
---|
Diameter | 2.5,3.2,4,5,6.3,7,8 |
---|
Length | NON |
---|