Metric Coarse Hexagon Turnbuckle Body Steel DIN1479


dd2lmes maxs mind4
M6-30.000022.500011.050010.00009.78004.0000
M8-35.000025.000014.380013.000012.73004.0000
M10-45.000033.000017.770016.000015.73004.0000
M12-55.000040.000020.030018.000017.73004.0000
M16-75.000055.000026.750024.000023.67004.0000
?2021.000095.000024.000032.950030.000029.16004.0000
?2426.0000115.000029.000039.550036.000035.00004.0000
?3032.0000125.000036.000050.850046.000045.00004.0000

Metric Coarse Hexagon Turn buckle Body Steel DIN 1479