Metric Coarse Two Knurled Closed Long Male Extension Thread Inserts For Plastic Moulding Steel DIN16903U
SKU:
2062
Details
Details
Metric Coarse Two Knurled Closed Long Male Extension Thread Inserts For Plastic Moulding Steel DIN16903U
M | L | L.g |
---|
M4 | 8 | 11 |
M5 | 10 | 13.3 |
M6 | 12 | 15.8 |
M8 | 16 | 20.6 |
M10 | 20 | 25 |
M12 | 24 | 29.8 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | STEEL |
---|
Standard Number | DIN16903U |
---|
Second Standard | - |
---|
Drive | Knurled |
---|
Head | NON |
---|
American Generic Brand Term | BUSH |
---|
Diameter | M4,M5,M6,M8,M10,M12 |
---|