Metric Coarse Two Hexagon Closed Thread Inserts For Plastic Moulding Brass DIN16903P
| M | L | L.g |
|---|---|---|
| M3 | 3 | 5.5 |
| M4 | 4 | 7 |
| M5 | 5 | 8.3 |
| M6 | 6 | 9.3 |
| M8 | 8 | 12.6 |
| M10 | 10 | 15.0000 |
| M12 | 12 | 17.8000 |
| Weight | 0.0000 |
|---|---|
| Material | BRASS |
| Standard Number | DIN16903P |
| Second Standard | - |
| Drive | Hexagon |
| Head | NON |
| American Generic Brand Term | BUSH |
| Diameter | M3,M4,M5,M6,M8,M10,M12 |
| Length | NON |