BoretDC1bLhGWn
80.808.703.001.102.401.008.400.900.60
90.809.803.701.302.501.009.400.900.60
101.0010.803.301.403.201.2010.401.100.60
111.0011.804.101.503.301.2011.401.100.60
121.0013.004.901.703.401.5012.501.100.80
131.0014.105.401.803.601.5013.601.100.90
141.0015.106.201.903.701.7014.601.100.90
151.0016.207.202.003.701.7015.701.101.10
161.0017.308.002.003.801.7016.801.101.20
171.0018.308.802.103.901.7017.801.101.20
181.0019.509.402.204.102.0019.001.101.50
191.0020.5010.402.204.102.0020.001.101.50
201.0021.5011.202.304.202.0021.001.101.50
211.0022.5012.202.404.202.0022.001.101.50
221.0023.5013.202.504.202.0023.001.101.50
231.2024.6014.202.504.202.0024.101.301.50
241.2025.9014.802.604.402.0025.201.301.80
251.2026.9015.502.704.502.0026.201.301.80
261.2027.9016.102.804.702.0027.201.301.80
271.2029.1017.102.904.702.0028.401.302.10
281.2030.1017.902.904.802.0029.401.302.10
291.2031.1018.403.004.802.0030.401.302.10
301.2032.1019.903.004.802.0031.401.302.10
311.2033.4020.003.205.202.5032.701.302.60
321.2034.4020.603.205.402.5033.701.302.60
331.2035.5021.603.305.402.5034.701.302.60
341.5036.5022.603.305.402.5035.701.602.60
351.5037.8023.603.405.402.5037.001.603.00
361.5038.8024.603.505.402.5038.001.603.00
371.5039.8025.403.605.502.5039.001.603.00
381.5040.8026.403.705.502.5040.001.603.00
391.5042.0027.203.805.602.5041.001.603.00
401.7543.5027.803.905.802.5042.501.853.80
411.7544.5028.604.005.902.5043.501.853.80
421.7545.5029.604.105.902.5044.501.853.80
431.7546.5030.604.205.902.5045.501.853.80
441.7547.5031.404.206.002.5046.501.853.80
451.7548.5032.004.306.202.5047.501.853.80
461.7549.5032.704.406.302.5048.501.853.80
471.7550.5033.504.406.402.5049.501.853.80
481.7551.5034.504.506.402.5050.501.853.80
502.0054.2036.304.606.502.5053.002.154.50
512.0055.2037.304.706.502.5054.002.154.50
522.0056.2037.904.706.702.5055.002.154.50
532.0057.2038.904.906.702.5056.002.154.50
542.0058.2039.905.006.702.5057.002.154.50
552.0059.2040.705.006.802.5058.002.154.50
562.0060.2041.705.106.802.5059.002.154.50
572.0061.2042.705.106.802.5060.002.154.50
582.0062.2043.505.206.902.5061.002.154.50
602.0064.2044.705.407.302.5063.002.154.50
622.0066.2046.705.507.302.5065.002.154.50
632.0067.2047.705.607.302.5066.002.154.50
642.0068.2048.205.707.502.5067.002.154.50
652.5069.2049.005.807.603.0068.002.654.50
672.5071.5050.806.007.703.0070.002.654.50
682.5072.5051.606.107.803.0071.002.654.50
702.5074.5053.606.207.803.0073.002.654.50
722.5076.5055.606.407.803.0075.002.654.50
752.5079.5058.606.607.803.0078.002.654.50
782.5082.5060.106.808.503.0081.002.654.50
802.5085.5062.107.008.503.0083.502.655.30
822.5087.5064.107.008.503.0085.502.655.30
853.0090.5066.907.208.603.5088.503.155.30
873.0092.5068.907.308.603.5090.503.155.30
883.0093.5069.907.408.603.5091.503.155.30
903.0095.5071.907.608.603.5093.503.155.30
923.0097.5073.707.808.703.5095.503.155.30
953.00100.5076.508.108.803.5098.503.155.30
973.00102.5078.508.208.803.50100.503.155.30
983.00103.5079.008.309.003.50101.503.155.30
1003.00105.5080.608.409.203.50103.503.155.30
1024.00108.0082.008.509.503.50106.004.156.00
1054.00112.0085.008.709.503.50109.004.156.00
1084.00115.0088.008.909.503.50112.004.156.00
1104.00117.0088.209.0010.403.50114.004.156.00
1124.00119.0090.009.1010.503.50116.004.156.00
1154.00122.0093.009.3010.503.50119.004.156.00
1204.00127.0096.909.7011.003.50124.004.156.00
1254.00132.00101.9010.0011.004.00129.004.156.00
1304.00137.00106.9010.2011.004.00134.004.156.00
1354.00142.00111.5010.5011.204.00139.004.156.00
1404.00147.00116.5010.7011.204.00144.004.156.00
1454.00152.00121.0010.9011.404.00149.004.156.00
1504.00158.00124.8011.2012.004.00155.004.157.50
1554.00164.00129.8011.4012.004.00160.004.157.50
1604.00169.00132.7011.6013.004.00165.004.157.50
1654.00174.50137.7011.8013.004.00170.004.157.50
1704.00179.50141.6012.2013.504.00175.004.157.50
1754.00184.50146.6012.7013.504.00180.004.157.50
1804.00189.50150.2013.2014.204.00185.004.157.50
1854.00194.50155.2013.7014.204.00190.004.157.50
1904.00199.50160.2013.8014.204.00195.004.157.50
1954.00204.50165.2013.8014.204.00200.004.157.50
2004.00209.50170.2014.0014.204.00205.004.157.50
2055.00217.00175.2014.0014.204.00211.005.159.00
2105.00222.00180.2014.0014.204.00216.005.159.00
2155.00227.00185.2014.0014.204.00221.005.159.00
2205.00232.00190.2014.0014.204.00226.005.159.00
2255.00237.00195.2014.0014.204.00231.005.159.00
2305.00242.00200.2014.0014.204.00236.005.159.00
2355.00247.00205.2014.0014.204.00241.005.159.00
2405.00252.00210.2014.0014.204.00246.005.159.00
2455.00257.00215.2014.0014.204.00251.005.159.00
2505.00262.00220.2014.0014.204.00256.005.159.00
2555.00270.00221.0016.0016.205.00263.005.1512.00
2605.00275.00226.0016.0016.205.00268.005.1512.00
2655.00280.00231.0016.0016.205.00273.005.1512.00
2705.00285.00236.0016.0016.205.00278.005.1512.00
2755.00290.00241.0016.0016.205.00283.005.1512.00
2805.00295.00246.0016.0016.205.00288.005.1512.00
2855.00300.00251.0016.0016.205.00293.005.1512.00
2905.00305.00256.0016.0016.205.00298.005.1512.00
2955.00310.00261.0016.0016.205.00303.005.1512.00
3005.00315.00266.0016.0016.205.00308.005.1512.00
3106.00327.00268.0020.0020.206.00320.006.2015.00
3206.00337.00278.0020.0020.206.00330.006.2015.00
3306.00347.00288.0020.0020.206.00340.006.2015.00
3406.00357.00298.0020.0020.206.00350.006.2015.00
3506.00367.00308.0020.0020.206.00360.006.2015.00
3606.00377.00318.0020.0020.206.00370.006.2015.00
3706.00387.00328.0020.0020.206.00380.006.2015.00
3806.00397.00338.0020.0020.206.00390.006.2015.00
3906.00407.00348.0020.0020.206.00400.006.2015.00
4006.00417.00358.0020.0020.206.00410.006.2015.00