The DNH Series Spirolox Retaining Ring is Smalley's equivalent to the European or "Hard" metric retaining ring series. With their 2-turn offset configuration, these spiral rings will fit into the grooves established by DIN specifications.

Standard Materials:

Carbon Steel / 302 & 316 Stainless Steel. Add suffix “-S02” or “-S16” for stainless steel


Part NumberHousing Diameter Ring Outside Diameter  Ring Radial Wall Min  Ring Radial Wall Max  Ring Thickness  Groove Diameter  Groove Width Groove Yield  (1)Ring Shear (2)
XEH-66         6.35         0.33         0.53         0.38         6.30         0.514401,880
XEH-77         7.37         0.33         0.53         0.38         7.32         0.515502,190
XEH-88         8.51         0.51         0.71         0.38         8.43         0.518402,500
XEH-99         9.60         0.64         0.84         0.64         9.50         0.741,1004,740
XEH-1010       10.62         0.64         0.84         0.64       10.52         0.741,2705,270
XEH-1111       11.79         0.76         0.96         0.64       11.71         0.741,9005,790
XEH-1212       12.89         1.02         1.22         0.60       12.70         0.702,0507,950
XEH-1313       13.95         1.02         1.22         0.89       13.75         1.002,41012,110
XEH-1414       15.07         1.27         1.47         0.89       14.85         1.002,93013,040
XEH-1515       16.14         1.27         1.47         0.89       15.90         1.003,29013,970
XEH-1616       17.15         1.27         1.47         0.89       16.95         1.003,74014,900
XEH-1717       18.32         1.52         1.73         0.89       18.05         1.004,39015,830
XEH-1818       19.39         1.52         1.73         0.89       19.10         1.004,82016,760
XEH-1919       20.48         1.52         1.73         0.89       20.17         1.005,46017,690
XEH-2020       21.51         1.78         1.98         0.89       21.22         1.005,94018,620
XEH-2121       22.56         1.78         1.98         0.89       22.27         1.006,55019,550
XEH-2222       23.65         1.78         1.98         1.07       23.37         1.207,39024,630
XEH-2323       24.69         2.03         2.24         1.07       24.42         1.207,95025,750
XEH-2424       25.73         2.03         2.24         1.07       25.47         1.208,65026,870
XEH-2525       27.03         2.03         2.24         1.07       26.67         1.2010,23027,990
XEH-2626       28.07         2.03         2.24         1.07       27.77         1.2011,27029,110
XEH-2727       29.11         2.49         2.69         1.27       28.87         1.4012,36031,170
XEH-2828       30.10         2.49         2.69         1.27       29.87         1.4012,82032,330
XEH-2929       31.21         2.49         2.69         1.27       30.95         1.4013,84033,480
XEH-3030       32.28         2.49         2.69         1.27       32.00         1.4014,61034,640
XEH-3131       33.32         2.49         2.69         1.27       33.05         1.4015,55035,790
XEH-3232       34.23         2.49         2.69         1.27       34.00         1.4015,88036,950
XEH-3434       36.46         2.87         3.07         1.27       36.20         1.4018,21039,260
XEH-3535       37.55         2.87         3.07         1.27       37.30         1.4019,60040,410
XEH-3636       38.68         2.87         3.07         1.27       38.40         1.4021,04041,560
XEH-3737       39.60         2.87         3.07         1.27       39.40         1.4021,62042,720
XEH-3838       40.77         2.87         3.07         1.27       40.50         1.4023,13043,870
XEH-4040       42.91         3.12         3.33         1.57       42.50         1.7524,35057,090
XEH-4242       45.01         3.12         3.33         1.57       44.60         1.7526,59059,950
XEH-4545       48.13         3.12         3.33         1.57       47.70         1.7529,59064,230
XEH-4646       49.28         3.12         3.33         1.57       48.80         1.7531,37065,660
XEH-4747       50.32         3.89         4.09         1.57       49.90         1.7533,19067,080
XEH-4848       51.46         3.89         4.09         1.57       51.00         1.7535,07068,510
XEH-5050       53.66         3.89         4.09         1.57       53.20         1.7538,96071,370
XEH-5252       54.30         3.12         3.33         1.25       53.79         1.4222,79059,090
XEH-5353       55.32         3.12         3.33         1.25       54.79         1.4223,23060,230
XEH-5555       57.38         3.38         3.58         1.25       56.85         1.4224,91062,500
XEH-5656       58.40         3.38         3.58         1.25       57.85         1.4225,36063,640
XEH-5858       60.43         3.38         3.58         1.25       59.85         1.4226,27065,910
XEH-5959       61.54         3.38         3.58         1.25       60.93         1.4227,87067,050
XEH-6060       62.57         3.38         3.58         1.25       61.99         1.4229,22068,180