Metric Tab Locking Washer Steel BS5814

SKU: 2528
Details
Details

Metric Tab Locking Washer Steel bs5814

sizeM 4M 5M 6M 8M 10M 12M 14M 16M 20M 24M 30
d 1 (Max)4.235.236.238.2710.2712.3014.3016.3020.3824.3830.38
d 1 (Min)4.055.056.058.0510.0512.0514.0516.0520.0524.0530.05
d 2 (Max)9.0010.0012.5017.0021.0024.0028.0030.0037.0044.0056.00
d 2 (Min)8.709.7012.1016.6020.5023.5027.5029.5036.2043.2055.00
S (Max)1.071.071.071.281.281.281.281.281.681.681.68
S (Min)0.930.930.931.121.121.121.121.121.521.521.52
a + 0.25 05.005.506.508.0010.5012.0014.0016.0020.0024.0030.00
b + 0.25 07.008.009.0011.0014.0016.0018.0019.0023.0027.0035.00
c + 0.25 04.004.205.606.609.0010.3011.5012.7015.0019.0024.50
e -+ 0.252.503.004.005.006.007.008.009.0011.0013.5017.50
f -+ 0.250.400.500.601.001.201.301.301.301.302.502.50
g -+ 2 degree6060606060808080909595
h 0 - 0.123.003.003.004.004.004.904.904.906.008.208.20
j 0 - 0.252.402.502.502.503.803.803.803.803.803.804.50
k -+ 0.206.106.607.5010.2012.0013.5015.8016.7020.3026.0032.00
l -+ 0.205.005.506.007.5010.0011.0013.0014.0017.5021.5027.00
m -+ 0.301.001.001.001.301.301.301.301.902.502.502.50
n -+ 0.251.001.001.001.001.001.301.301.301.501.501.50