Metric Flat Washer For Sems Machine Screws Type L Steel-200Hv ISO10644

SKU: 2303
Details
Details
Metric Flat Washer For Sems Machine Screws Type L Steel-200Hv ISO10644
dd1 mind1 maxd2 maxd2 minh nomh maxh min
21.75001.85006.00005.70000.60000.65000.5500
2.52.25002.35008.00007.64000.60000.65000.5500
32.75002.85009.00008.64000.80000.85000.7500
3.53.20003.320011.000010.57000.80000.85000.7500
43.60003.720012.000011.57001.00001.06000.9400
54.55004.670015.000014.57001.00001.06000.9400
65.50005.620018.000017.57001.60001.68001.5200
87.40007.550024.000023.48002.00002.09001.9100
109.30009.520030.000029.48002.50002.60002.4000
1211.000011.270037.000036.38003.00003.11002.8900
Additional Info
Additional Info
Weight0.0000
MaterialSteel-200Hv
Standard NumberISO10644
Second Standard-
DriveNon
HeadNON
American Generic Brand TermSEMS
Diameter M2,M2.5,M3,M3.5,M4,M5,M6,M8,M10,M12
LengthNON