did minid maxod minod maxt mint max
M12  14.00  14.43  25.70  27.00    3.10    4.60
M16  18.00  18.43  32.40  34.00    3.10    4.60
M20  22.00  22.52  37.40  39.00    3.10    4.60
M24  26.00  26.52  48.40  50.00    3.40    4.60
M30  33.00  33.62  58.10  60.00    3.40    4.60
M36  39.00  39.62  70.10  72.00    3.40    4.60

 

Metric Hardened 35/45 HRC Structural Steel Washer AS1252 with identification tabs AS 1252 high strength