Dd1d2h
M55.500015.00001.6000
M66.600018.00002.0000
M77.600021.00002.0000
M89.000024.00002.0000
M1011.000030.00002.5000
M1214.000036.00003.0000
M1416.000042.00003.0000
M1618.000048.00004.0000
M1820.000054.00004.0000
M2022.000060.00005.0000
M2224.000066.00005.0000
M2426.000072.00006.0000
M2730.000081.00006.0000
M3033.000090.00008.0000
M3336.000099.00008.0000
M3639.0000108.000010.0000
M3942.0000117.000010.0000