Schnorr Metric Conical Spring Safety Load Washer HDS Spring-Steel C60S DIN6796

SKU: 2709
Details
Details

Schnorr heavy duty load washers HDS washers have been specifically developed for high-strength bolts in the strength classes 8.8 and 10.9. The Loads of the washers have been matched to these bolts and are 70 to 90% of the bolt load in the flat state. 

These high loads naturally require large cross-sections, which is why the outside diameter of the load washer is considerably larger than that of the Schnorr serrated safety washer. As a result, the area required for a design with load washers cannot be ignored. 

As a highly progressive load increase occurs at the end of the spring deflection when the washer is flattened and conform to DIN 6796

dd1d2sh maxh min
2          2.20 5          0.40           0.50           0.60
2.5          2.70 6          0.50           0.60           0.72
3          3.20 7          0.60           0.70           0.85
3.5          3.70 8          0.80           0.90           1.06
4          4.30 9          1.00           1.10           1.30
5          5.30 11          1.20           1.30           1.55
6          6.40 14          1.50           1.70           2.00
7          7.40 17          1.75           2.00           2.30
8          8.40 18          2.00           2.20           2.60
10        10.50 23          2.50           2.80           3.20
12        13.00 29          3.00           3.40           3.95
14        15.00 35          3.50           4.00           4.65
16        17.00 39          4.00           4.60           5.25
18        19.00 42          4.50           5.10           5.80
20        21.00 45          5.00           5.60           6.40
22        23.00 49          5.50           6.10           7.05
24        25.00 56          6.00           6.80           7.75
27        28.00 60          6.50           7.30           8.35
30        31.00 70          7.00           8.00           9.20

 

Schnorr Metric Conical Spring Safety Load Washer HDS Spring-Steel C60S  DIN6796 din 6796 sku2709