Schnorr Metric Conical Spring Safety Load Washer HDS Spring-Steel C60S DIN6796
Schnorr heavy duty load washers HDS washers have been specifically developed for high-strength bolts in the strength classes 8.8 and 10.9. The Loads of the washers have been matched to these bolts and are 70 to 90% of the bolt load in the flat state.
These high loads naturally require large cross-sections, which is why the outside diameter of the load washer is considerably larger than that of the Schnorr serrated safety washer. As a result, the area required for a design with load washers cannot be ignored.
As a highly progressive load increase occurs at the end of the spring deflection when the washer is flattened and conform to DIN 6796
d | d1 | d2 | s | h max | h min |
2 | 2.20 | 5 | 0.40 | 0.50 | 0.60 |
2.5 | 2.70 | 6 | 0.50 | 0.60 | 0.72 |
3 | 3.20 | 7 | 0.60 | 0.70 | 0.85 |
3.5 | 3.70 | 8 | 0.80 | 0.90 | 1.06 |
4 | 4.30 | 9 | 1.00 | 1.10 | 1.30 |
5 | 5.30 | 11 | 1.20 | 1.30 | 1.55 |
6 | 6.40 | 14 | 1.50 | 1.70 | 2.00 |
7 | 7.40 | 17 | 1.75 | 2.00 | 2.30 |
8 | 8.40 | 18 | 2.00 | 2.20 | 2.60 |
10 | 10.50 | 23 | 2.50 | 2.80 | 3.20 |
12 | 13.00 | 29 | 3.00 | 3.40 | 3.95 |
14 | 15.00 | 35 | 3.50 | 4.00 | 4.65 |
16 | 17.00 | 39 | 4.00 | 4.60 | 5.25 |
18 | 19.00 | 42 | 4.50 | 5.10 | 5.80 |
20 | 21.00 | 45 | 5.00 | 5.60 | 6.40 |
22 | 23.00 | 49 | 5.50 | 6.10 | 7.05 |
24 | 25.00 | 56 | 6.00 | 6.80 | 7.75 |
27 | 28.00 | 60 | 6.50 | 7.30 | 8.35 |
30 | 31.00 | 70 | 7.00 | 8.00 | 9.20 |
Schnorr Metric Conical Spring Safety Load Washer HDS Spring-Steel C60S DIN6796 din 6796 sku2709