Metric American Flat Washer Wide Stainless-Steel 18/8-304-A2 B18.22M
Loading...
Zoom

Metric American Flat Washer Wide Stainless-Steel 18/8-304-A2 B18.22M

SKU: 1319
Details
Details
Metric American Flat Washer Wide Stainless-Steel 18/8-304-A2 B18.22M
D d1 Max d1 Min d2 Max d2 Min h Max h Min
M1.62.09001.95006.00005.70000.90000.6000
M22.64002.50008.00007.64000.90000.6000
M2.53.14003.000010.00009.64001.20000.8000
M33.68003.500012.000011.57001.40001.0000
M3.54.18004.000015.000014.57001.75001.2000
M44.88004.700016.000015.57002.30001.6000
M55.78005.500020.000019.48002.30001.6000
M66.87006.650025.400024.88002.30001.6000
M89.12008.900032.000031.38002.80002.0000
M1011.120010.850039.000038.38003.50002.5000
M1213.570013.300044.000043.38003.50002.5000
M1415.520015.250050.000049.38004.00003.0000
M1617.520017.250056.000054.80004.80003.5000
M2022.320021.800066.000064.80005.10004.0000
M2426.120025.600072.000070.80005.60004.5000
M3033.020032.400090.000088.60006.40005.0000
M3638.920038.3000110.0000108.60008.50007.0000