Technical Information
Fastener Specific
Supply Source

schnorr Metric Conical Ribbed Locking Washer S Light Stainless-Steel X5CrNi18-10 1-4301
Loading...
Zoom

schnorr Metric Conical Ribbed Locking Washer S Light Stainless-Steel X5CrNi18-10 1-4301

SKU: 1510
Details
Details

 

h max:  Maximum dimension as delivered   h min:   Minimum dimension after the load test

mm nom inchd1d2sh minh max
1.6           1.70          3.20          0.35          0.40          0.60
2           2.20          4.00          0.35          0.40          0.60
2.5           2.70          4.80          0.45          0.50          0.90
31/8"          3.20          5.50          0.45          0.50          0.90
3.5           3.70          6.00          0.45          0.55          0.90
45/32"          4.30          7.00          0.50          0.55          1.00
53/16"          5.30          9.00          0.60          0.60          1.10
6           6.40        10.00          0.60          0.70          1.20
6.351/4"          6.70          9.50          0.60          0.65          1.20
7           7.40        12.00          0.70          0.80          1.30
85/16"          8.40        13.00          0.70          0.90          1.40
103/8"        10.50        16.00          0.90          1.10          1.60
11.17/16"        11.60        15.90          0.90          1.05          1.60
12         13.00        18.00          1.00          1.15          1.70
12.71/2"        13.70        19.00          1.00          1.25          1.80
14         15.00        22.00          1.10          1.35          2.00
165/8"        17.00        24.00          1.30          1.55          2.10
18         19.00        27.00          1.40          1.75          2.30
193/4"        20.00        30.00          1.40          1.90          2.50
20         21.00        30.00          1.40          1.85          2.50
227/8"        23.00        33.00          1.40          1.95          2.70
24         25.60        36.00          1.60          2.15          2.90
25.41"        27.00        38.00          1.80          2.35          3.10
27         28.60        39.00          1.80          2.35          3.10
301.1/8"        31.60        45.00          1.80          2.60          3.60
361.3/8"        38.00        54.00          2.50          3.20          4.20

 

 

schnorr Metric Conical Ribbed Locking Washer S Light Stainless-Steel X5CrNi18-10 1-4301 DIN9250S

 

 

 

Additional Info
Reviews