Inch Fender Washer Stainless-Steel 18/8-304-A2
Inch Fender Washer Stainless-Steel 18/8-304-A2
D | d1 | d2 | h max | h min |
---|---|---|---|---|
No 10" | 7/32" | 1" | 0.0800 | 0.5100 |
1/4" | 9/32" | 1" | 0.0800 | 0.5100 |
1/4" | 9/32" | 1.1/4" | 0.0800 | 0.5100 |
1/4" | 9/32" | 1-1/2" | 0.0800 | 0.5100 |
5/16" | 11/32" | 1-1/4" | 0.0800 | 0.5100 |
5/16" | 11/32" | 1-1/2" | 0.0800 | 0.5100 |
3/8" | 13/32" | 1-1/4" | 0.0800 | 0.5100 |
3/8" | 13/32" | 1-1/2" | 0.0800 | 0.5100 |
1/2" | 17/32" | 2" | 0.0800 | 0.5100 |