UNC Socket Countersunk Screw Aluminium B18.3
D | d max | d min | dk min | k ref | s nom | y min |
---|---|---|---|---|---|---|
No.0 | 0.0600 | 0.0568 | 0.1170 | 0.0440 | 0.0350 | 0.0250 |
No.1 | 0.0730 | 0.0695 | 0.1430 | 0.0540 | 0.0500 | 0.0310 |
No.2 | 0.0860 | 0.0822 | 0.1680 | 0.0640 | 0.0500 | 0.0380 |
No.3 | 0.0990 | 0.0949 | 0.1930 | 0.0730 | 1/16" | 0.0440 |
No.4 | 0.1120 | 0.1075 | 0.2180 | 0.0830 | 1/16" | 0.0550 |
No.5 | 0.1250 | 0.1202 | 0.2400 | 0.0900 | 5/64" | 0.0360 |
No.6 | 0.1380 | 0.1329 | 0.2630 | 0.0970 | 5/64" | 0.0660 |
No.8 | 0.1640 | 0.1585 | 0.3110 | 0.1120 | 3/32" | 0.0760 |
No.10 | 0.1900 | 0.1840 | 0.3590 | 0.1270 | 1/8" | 0.0870 |
1/4" | 0.2500 | 0.2435 | 0.4800 | 0.1610 | 5/32" | 0.1110 |
5/16" | 0.3125 | 0.3053 | 0.6000 | 0.1980 | 3/16" | 0.1350 |
3/8" | 0.3750 | 0.3678 | 0.7200 | 0.2340 | 7/32" | 0.1590 |
7/16" | 0.4375 | 0.4294 | 0.7810 | 0.2340 | 1/4" | 0.1590 |
1/2" | 0.5000 | 0.4919 | 0.8720 | 0.2510 | 5/16" | 0.1720 |
5/8" | 0.6250 | 0.6163 | 1.1120 | 0.3240 | 3/8" | 0.2200 |
3/4" | 0.7500 | 0.7406 | 1.3550 | 0.3960 | 1/2" | 0.2200 |
7/8" | 0.8750 | 0.8647 | 1.6040 | 0.4680 | 9/16" | 0.2480 |
1" | 1.0000 | 0.9886 | 1.8410 | 0.5400 | 5/8" | 0.2970 |
1.1/8" | 1.1250 | 1.1086 | 2.0790 | 0.6110 | 3/4" | 0.3250 |
1.1/4" | 1.2500 | 1.2336 | 2.3160 | 0.6830 | 7/8" | 0.3580 |
1.3/8" | 1.3750 | 1.3566 | 2.5530 | 0.7550 | 7/8" | 0.4020 |
1.1/2" | 1.5000 | 1.4818 | 2.7910 | 0.8270 | 1." | 0.4350 |