UNC socket cap screw
Socket Capscrews
Inch Unc socket cap screws are to American specification ANSI B18.3 and have a hardness of RC38/43 within the same range of a 12.9 socket cap
For more detail LINK
UNC Socket Cap Screw 1960 Brass B18.3
UNC Socket Cap Screw 1960 Aluminium B18.3
UNC Socket Cap Screw 1960 Monel B18.3
UNC Socket Cap Screw 1960 Nylon-66 B18.3
UNC Socket Cap Screw 1960 Phosphor-Bronze B18.3
UNC Socket Cap Screw 1936 Stainless-Steel 18/8-304-A2 BS2470
UNC Socket Cap Screw 1960 Stainless-Steel 18/8-304-A2 B18.3
UNC Socket Cap Screw 1960 Grade-12.9, Rc38/43 B18.3
UNC Socket Cap Screw 1936 Grade-12.9 BS2470
UNC Socket Cap Screw 1960 Full Thread Grade-12.9, Rc38/43 B18.3