BSW Whitworth Socket Button Head Screw Grade-T(10.9)
Loading...
Zoom

BSW Whitworth Socket Button Head Screw Grade-T(10.9)

SKU: 1681
Details
Details
BSW Whitworth Socket Button Head Screw Grade-T(10.9)
ddk maxb max e max k max g maxr noms key t min
3/16"0.36100.18800.18600.10100.02000.21801/8"1.0000
1/4"0.43700.25000.23200.13200.03100.25405/32"1.0000
5/16"0.54700.31300.26800.16600.03100.31403/16"1.0000
3/8"0.65600.37500.30400.19900.03100.37307/32"1.2500
7/16"0.75000.43800.34000.23200.03100.41701/4"1.5000
1/2"0.87500.50000.41400.26500.04600.48605/16"2.0000
5/8"1.00000.62500.48600.33100.06200.52803/8"2.0000
3/4"1.21800.75000.61300.39800.07800.67001/2"2.0000