d | dk max | b max | e max | k max | g max | r nom | s key | t min |
---|---|---|---|---|---|---|---|---|
3/16" | 0.3610 | 0.1880 | 0.1860 | 0.1010 | 0.0200 | 0.2180 | 1/8" | 1.0000 |
1/4" | 0.4370 | 0.2500 | 0.2320 | 0.1320 | 0.0310 | 0.2540 | 5/32" | 1.0000 |
5/16" | 0.5470 | 0.3130 | 0.2680 | 0.1660 | 0.0310 | 0.3140 | 3/16" | 1.0000 |
3/8" | 0.6560 | 0.3750 | 0.3040 | 0.1990 | 0.0310 | 0.3730 | 7/32" | 1.2500 |
7/16" | 0.7500 | 0.4380 | 0.3400 | 0.2320 | 0.0310 | 0.4170 | 1/4" | 1.5000 |
1/2" | 0.8750 | 0.5000 | 0.4140 | 0.2650 | 0.0460 | 0.4860 | 5/16" | 2.0000 |
5/8" | 1.0000 | 0.6250 | 0.4860 | 0.3310 | 0.0620 | 0.5280 | 3/8" | 2.0000 |