Dn maxn minn nomt mindt
M10.40000.26000.33000.4000 
M1.20.40000.26000.33000.4000 
M1.40.40000.26000.33000.4800 
M1.60.45000.31000.38000.5600 
M20.45000.31000.38000.6400 
M2.50.60000.46000.53000.7200 
M30.60000.46000.53000.8000 
M3.50.70000.56000.63000.9600 
M40.80000.66000.73001.1200 
M51.00000.86000.93001.2800 
M61.20001.06001.13001.6000 
M81.51001.26001.38502.0000 
M101.91001.66001.78502.4000 
M122.30002.10002.20002.8000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A1
Standard NumberDIN553
Second StandardISO7434
DriveSlot
HeadNON
American Generic Brand TermGRUB
Diameter M1,M1.2,M1.4,M1.6,M2,M2.5,M3,M3.5,M4,M5,M6,M8,M10,M12
Length2,3,4,5,6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50