Technical Information
Fastener Specific
Supply Source

UNC Socket Set Jam Screw Steel

SKU: 1858
Details
Details
UNC Socket Set Jam Screw Steel
ddjjL nomL maxL min
No.40.11200.05000.05000.07800.08800.0680
No.50.12501/16”0.06200.09400.10300.0830
No.60.13801/16”0.06200.09400.10300.0830
No.80.16405/64”0.07800.10900.11900.0990
No.100.19003/32”0.09400.12500.13500.1150
1/4”0.25001/8”0.12500.12500.13500.1150
5/16”0.31255/32”0.15600.15600.16600.1460
3/8”0.37503/16”0.18800.18800.19700.1770
7/16”0.43757/32”0.21900.21900.22800.2080
1/2”0.50001/4”0.25000.25000.26000.2400
5/8”0.62505/16”0.31200.31200.32200.3020
3/4”0.75003/8”0.37500.37500.38500.3650
7/8”0.87501/2”0.50000.43800.44700.4270
1”1.00009/16”0.56200.50000.51000.4900
Additional Info
Reviews
Tags