Metric Fine Socket Button Head Screw Grade-10.9 ISO7380
Loading...
Zoom

Metric Fine Socket Button Head Screw Grade-10.9 ISO7380

SKU: 1665
Details
Details

Metric Fine Socket Button Head Screw Grade-10.9 ISO7380


D        dk             k                  t                      s              
M23.70001.30000.70001.2500
M2.54.35001.40000.85001.5000
M35.70001.65001.04002.0000
M47.60002.20001.30002.5000
M59.50002.75001.56003.0000
M610.50003.30002.08004.0000
M814.00004.40002.60005.0000
M1017.50005.50003.12006.0000
M1221.00006.60004.16008.0000
M1628.00008.80005.200010.0000

 

 

Metric Fine thread Socket allen  Button Head Screw Grade-10.9 ISO7380 iso 7380