Dds nomt mindp maxdp ming maxg min
3/16”0.18753/32”0.07500.12700.12000.04900.0410
1/4”0.25001/8”0.10000.15600.14900.06700.0590
5/16”0.31255/32”0.12500.20300.19500.08200.0740
3/8”0.37503/16”0.15000.25000.24100.09900.0890
7/16”0.43757/32”0.17500.29700.28700.11400.1040
1/2”0.50001/4”0.20000.34400.33400.13000.1200
5/8”0.62505/16”0.25000.46900.45600.16400.1480
3/4”0.75003/8”0.30000.56200.54900.19600.1800
7/8”0.87501/2”0.40000.65600.64200.22700.2110
1”1.00009/16”0.45000.75000.73400.26000.2400