Technical Information
Fastener Specific
Supply Source

BA Socket Countersunk Screw Stainless-Steel 18/8-304-A2 BS2470
Loading...
Zoom

BA Socket Countersunk Screw Stainless-Steel 18/8-304-A2 BS2470

SKU: 1717
Details
Details
BA Socket Countersunk Screw Stainless-Steel 18/8-304-A2 BS2470
Dd maxdk maxdk mink noms nomt min
8BA0.08700.00000.14700.03800.05000.0300
6BA0.11020.21100.18300.05200.05000.0350
5BA0.12600.23900.21000.05801/16”0.0420
4BA0.14170.26900.23600.06601/16”0.0470
3BA0.16140.30700.26900.07505/64”0.0550
2BA0.18500.35100.31000.08603/32”0.0620
1BA0.20870.39600.35000.09703/32”0.0680
0BA0.23620.44900.39700.11001/8”0.0740
Additional Info
Reviews
Tags