Socket screw material alloying elements Manganese, Nickel, Chromium, Silicon, Titanium, Aluminium, Molybdenum, Vanadium and Copper can be added to steel to manipulate the steel's properties. The proportions of these elements will determine the properties of each socket screw alloy steel grade. When materials Molybdenum, Vanadium, Chromium or Nickel are added they create high strength steels and improve toughness; there is a high cost of adding these elements to the steel mix.
Along with Carbon and Alloy steel, there are Carbon-Boron steels. Small amounts of boron allow steels to be heat treated to high strengths without the cost penalty of other alloying elements, in many parts of the world there is widespread use of Boron steels for fasteners though there is some resistance in the USA because of historical failures. The properties of carbon-boron steels are not as good as alloy steels but they give a reasonable compromise between cost and improved properties benefits.
allen screws
UNC Slotted Grub (Set) Screw Flat Point Grade-14.9-45H B18.6.2
UNF Slotted Grub (Set) Screw Flat Point Grade-14.9-45H B18.6.2
Metric Fine Socket Cap Screw Grade-12.9 DIN912
Metric Coarse Socket Countersunk Screw Grade-8.8 DIN7991
Metric Coarse Socket Countersunk Screw Stainless-Steel-A2 DIN7991
Metric Coarse Socket Countersunk Screw Stainless-Steel-A4 DIN7991
Metric Coarse Socket Countersunk Screw Nylon-66 DIN7991
UNC Socket Countersunk Screw Stainless-Steel 18/8-304-A2 B18.3
UNC Socket Countersunk Screw Brass B18.3
UNC Socket Countersunk Screw Nylon-66 B18.3
UNC Socket Countersunk Screw Phosphor-Bronze B18.3
UNF Socket Countersunk Screw Stainless-Steel 18/10-316-A4 B18.3
UNF Socket Countersunk Screw Brass B18.3
UNF Socket Countersunk Screw Aluminium B18.3
UNF Socket Countersunk Screw Nylon-66 B18.3
UNF Socket Countersunk Screw Phosphor-Bronze B18.3
BSW Whitworth Socket Countersunk Screw Stainless-Steel 18/8-304-A2 BS2470
BSF Socket Countersunk Screw Grade-X(12.9) BS2470
BSF Socket Countersunk Screw Stainless-Steel 18/8-304-A2 BS2470
UNC Spline Socket Countersunk Screw Grade-12.9 B18.3
UNF Spline Socket Countersunk Screw Grade-12.9 B18.3
Metric Coarse Torx Socket Cap Screw Grade-12.9 ISO14579
Metric Coarse Torx Socket Cap Screw Steel ISO14579
Metric Coarse Torx Socket Cap Screw Stainless-Steel-A2 ISO14579
Metric Coarse Torx Low Head Socket Cap Screw Steel ISO14580
Metric Coarse Torx Socket Button Head Screw Steel
Metric Coarse Socket Flange Cap Screw Steel
UNC Socket Set Jam Screw Steel
UNC Socket Countersunk Screw Monel B18.3
BSW Whitworth Socket Countersunk Screw Grade-X(12.9) BS2470
BA Socket Countersunk Screw Grade-X(12.9) BS2470
Metric Coarse Set Screw Thrust Point Grade-5.8 Hard-End DIN6332
Metric Coarse Slotted Set Screw Thrust Point Grade-5.8 Hard-End DIN6332
Metric Coarse Socket Set Screw Thrust Point Grade-5.8 Hard-End DIN6332
Metric Hexagon Keys Short Arm Torx Steel
Metric Coarse External Torx Bolt with Flange Grade-8.8 DIN34800
Metric Coarse External Torx Bolt with Flange Grade-8.8 DIN34801
Metric Coarse Torx Socket Countersunk Screw Grade-10.9
Metric Coarse External Torx Bolt with Flange Grade-10.9 DIN34800
Metric Coarse External Torx Bolt with Flange Grade-10.9 DIN34801
Metric Coarse External Torx Bolt with Flange Grade-12.9 DIN34800
Metric Coarse External Torx Bolt with Flange Grade-12.9 DIN34801
Metric Coarse External Torx Bolt with Flange Stainless-Steel-A2 DIN34800
Metric Coarse External Torx Bolt with Flange Stainless-Steel-A2 DIN34801
Metric Coarse External Torx Bolt with Flange Stainless-Steel-A4 DIN34800
Metric Coarse External Torx Bolt with Flange Stainless-Steel-A4 DIN34801
Metric Coarse Torx Countersunk Head Machine Screw Grade-4.8 DIN965T
Metric Coarse Torx Countersunk Head Machine Screw Stainless-Steel-A2 DIN965T
Metric Coarse Torx Countersunk Head Machine Screw Stainless-Steel-A4 DIN965T
Metric Coarse External Torx Bolt with Flange Steel DIN34800
Metric Coarse Torx Raised Cheese Head Screw Steel DIN7985T
Metric Torx Countersunk Head Self Tapping Screw AB Case Hardened Steel DIN7982
Metric Torx Countersunk Head Self Tapping Screw B Case Hardened Steel DIN7982
Metric Torx Pan Head Self Tapping Screw B Case Hardened Steel DIN7981
UNC External Torx Bolt with Flange SAE-5(8.8) B18.2.1
UNC External Torx Bolt with Flange SAE-8(10.9) B18.2.1
UNC Torx Socket Countersunk Screw Grade-12.9 B18.3
UNC External Torx Bolt with Flange Stainless-Steel 18/8-304-A2 B18.2.1
UNC External Torx Bolt with Flange Stainless-Steel 18/10-316-A4 B18.2.1
UNF Torx Socket Countersunk Screw Grade-12.9 B18.3