Metric Coarse Wing Screw European Stainless-Steel-A4 DIN318

SKU: 586
Details
Details
Metric Coarse Wing Screw European Stainless-Steel-A4 DIN318
dj maxj minh maxh ming minm maxm min
M421.000019.000011.00009.00001.10004.60003.2000
M526.500024.500013.000011.00001.50006.00004.0000
M632.000029.000016.000014.00001.50007.00005.0000
M838.000035.000019.000017.00002.00008.50006.5000
M1050.000047.000024.000022.00003.600010.00008.0000
M1266.000063.000032.000029.00004.100013.000010.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A4
Standard NumberDIN318
Second Standard-
DriveWing
HeadNON
American Generic Brand TermTHUMB
Diameter M4,M5,M6,M8,M10,M12
Length6,8,10,16,20,30,35,40,50,60