UNC Square Head Set Screw Cup Point Alloy Steel B18.6.2
| D | D | G max | C max | C min | H max | H min | W nom | F max | F min |
|---|---|---|---|---|---|---|---|---|---|
| No.10 | 0.1900 | 0.2470 | 0.1020 | 0.8800 | 0.1480 | 0.1340 | 0.4800 | 0.1880 | 0.1800 |
| 1/4" | 0.2500 | 0.3310 | 0.1320 | 0.1180 | 0.1960 | 0.1780 | 0.6200 | 0.2500 | 0.2410 |
| 5/16" | 0.3120 | 0.4150 | 0.1720 | 0.1560 | 0.2450 | 0.2240 | 0.7800 | 0.3120 | 0.3020 |
| 3/8" | 0.3750 | 0.4970 | 0.2120 | 0.1940 | 0.2930 | 0.2700 | 0.9400 | 0.3750 | 0.3620 |
| 7/16" | 0.4370 | 0.5810 | 0.2520 | 0.2320 | 0.3410 | 0.3150 | 1.0900 | 0.4370 | 0.4230 |
| 1/2" | 0.5000 | 0.6650 | 0.2910 | 0.2700 | 0.3890 | 0.3610 | 1.2500 | 0.5000 | 0.4840 |
| 9/16" | 0.5620 | 0.6480 | 0.3320 | 0.3090 | 0.4370 | 0.4070 | 1.4100 | 0.5620 | 0.5450 |
| 5/8" | 0.6520 | 0.8330 | 0.3710 | 0.3470 | 0.4850 | 0.4520 | 1.5600 | 0.6250 | 0.6060 |
| 3/4" | 0.7500 | 1.0010 | 0.4500 | 0.4250 | 0.5820 | 0.5440 | 1.8800 | 0.7500 | 0.7290 |
| 7/8" | 0.8750 | 1.1700 | 0.5300 | 0.5020 | 0.6780 | 0.6350 | 2.1900 | 0.8750 | 0.8520 |
| 1" | 1.0000 | 1.3370 | 0.6090 | 0.5790 | 0.7740 | 0.7260 | 2.5000 | 1.0000 | 0.9740 |
| 1.1/8" | 1.1250 | 1.5050 | 0.6890 | 0.6550 | 0.8700 | 0.8170 | 2.8100 | 1.1250 | 1.0960 |
| 1.1/4" | 1.2500 | 1.6740 | 0.7670 | 0.7330 | 0.9660 | 0.9080 | 3.1200 | 1.2500 | 1.2190 |
| 1.3/8" | 1.3750 | 1.8430 | 0.8480 | 0.8080 | 1.0630 | 1.0000 | 3.4400 | 1.3750 | 1.3420 |
| 1.1/2" | 1.5000 | 2.0100 | 0.9260 | 0.8860 | 1.1590 | 1.0910 | 3.7500 | 1.5000 | 1.4640 |
| Weight | 0.0000 |
|---|---|
| Material | ALLOY STEEL |
| Standard Number | B18.6.2 |
| Second Standard | - |
| Drive | Square |
| Head | Square |
| American Generic Brand Term | TOOL POST |
| Diameter | 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2" |
| Length | 1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",5.1/4",5.1/2",5.3/4",6.",6.1/2",7.",7.1/2",8.",8.1/2",9.",9.1/2",10.",11.",12.",13.",14.",15.",16.",17.",18.",19.",20. |