D | dk | k | n | t | a | dp | l1 min | l1 max | l2 min | l2 max |
---|
M1.4 | 2.6000 | 0.8400 | 0.3000 | 0.4000 | 0.6000 | 0.8000 | 1.6000 | 2.5000 | 0.6000 | 1.0000 |
M1.6 | 3.0000 | 0.9600 | 0.4000 | 0.4500 | 0.7000 | 0.8000 | 2.0000 | 3.0000 | 1.0000 | 1.6000 |
M2 | 3.8000 | 1.2000 | 0.5000 | 0.6000 | 0.8000 | 1.2000 | 2.5000 | 4.0000 | 1.0000 | 2.0000 |
M2.5 | 4.7000 | 1.5000 | 0.6000 | 0.7000 | 0.9000 | 1.5000 | 3.0000 | 5.0000 | 1.6000 | 2.5000 |
M3 | 5.6000 | 1.6500 | 0.8000 | 0.8500 | 1.0000 | 2.0000 | 4.0000 | 6.0000 | 1.6000 | 3.0000 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | Grade-5.8 |
---|
Standard Number | DIN925 |
---|
Second Standard | - |
---|
Drive | Slot |
---|
Head | COUNTERSUNK |
---|
American Generic Brand Term | FLAT |
---|
Diameter | M1.4,M1.6,M2,M2.5,M3 |
---|
Length | 2,3,4,5,6,8,10,12,14,16 |
---|