Metric Coarse Pozi Countersunk Head Machine Screw Grade-4.8 DIN965
Loading...
Zoom

Metric Coarse Pozi Countersunk Head Machine Screw Grade-4.8 DIN965

SKU: 285
Details
Details

 

Ddk maxk
M1.63.00000.9600
M23.80001.2000
M2.54.70001.5000
M35.60001.6500
M3.56.50001.9300
M47.50002.2000
M59.20002.5000
M611.00003.0000
M814.50004.0000
M1018.00005.0000

Metric Coarse Pozi Countersunk Head Machine Screw Grade-4.8 DIN965

Metric Coarse Pozi Countersunk Head Machine Screw class 4.8 DIN 965 similar to ISO 7046