Metric Coarse Pozi Countersunk Head Machine Screw Stainless-Steel-A2 DIN965

SKU: 314
Details
Details
Metric Coarse Pozi Countersunk Head Machine Screw Stainless-Steel-A2 DIN965
Ddk maxk
M1.63.00000.9600
M23.80001.2000
M2.54.70001.5000
M35.60001.6500
M3.56.50001.9300
M47.50002.2000
M59.20002.5000
M611.00003.0000
M814.50004.0000
M1018.00005.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A2
Standard NumberDIN965
Second StandardISO7046
DrivePozi, Cross Recess
HeadCOUNTERSUNK
American Generic Brand Term-
Diameter M1.6,M2,M2.3,M2.5,M2.6,M3,M3.5,M4,M5,M6,M8,M10
Length3,4,5,6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60