Metric Coarse Phillips Countersunk Head Machine Screw Nylon-66 DIN965
SKU:
367
Details
Details
Metric Coarse Phillips Countersunk Head Machine Screw Nylon-66 DIN965
D | dk max | k |
---|
M1.6 | 3.0000 | 0.9600 |
M2 | 3.8000 | 1.2000 |
M2.5 | 4.7000 | 1.5000 |
M3 | 5.6000 | 1.6500 |
M3.5 | 6.5000 | 1.9300 |
M4 | 7.5000 | 2.2000 |
M5 | 9.2000 | 2.5000 |
M6 | 11.0000 | 3.0000 |
M8 | 14.5000 | 4.0000 |
M10 | 18.0000 | 5.0000 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | Nylon-66 |
---|
Standard Number | DIN965 |
---|
Second Standard | ISO7046 |
---|
Drive | Phillips |
---|
Head | COUNTERSUNK |
---|
American Generic Brand Term | - |
---|
Diameter | M1.6,M2,M2.3,M2.5,M2.6,M3,M3.5,M4,M5,M6,M8,M10 |
---|
Length | 3,4,5,6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60 |
---|