BSF Pozi Raised Cheese Head Machine Screw Grade-4.8 BS450
d | d | dk max | dk min | k nom | b max | b min |
---|
1/8” | 0.1250 | 0.2050 | 0.1870 | 0.0830 | 0.1200 | 0.1000 |
3/16” | 0.1875 | 0.3130 | 0.2920 | 0.1240 | 0.1800 | 0.1560 |
7/32” | 0.2188 | 0.3570 | 0.3340 | 0.1420 | 0.2050 | 0.1780 |
1/4” | 0.2500 | 0.4140 | 0.3890 | 0.1630 | 0.2370 | 0.2070 |
5/16” | 0.3125 | 0.5180 | 0.4900 | 0.1990 | 0.2950 | 0.2620 |
3/8” | 0.3750 | 0.6220 | 0.5900 | 0.2600 | 0.3550 | 0.3150 |
7/16” | 0.4375 | 0.6250 | 0.5890 | 0.2840 | 0.3680 | 0.3210 |
1/2” | 0.5000 | 0.7500 | 0.7100 | 0.3110 | 0.4120 | 0.3620 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | Grade-4.8 |
---|
Standard Number | BS450 |
---|
Second Standard | - |
---|
Drive | Pozi, Cross Recess |
---|
Head | RAISEDCHEESE |
---|
American Generic Brand Term | FILLISTER |
---|
Diameter | 0 |
---|
Length | 0 |
---|