BA Slotted Cheese Head Machine Screw Grade-4.8 BS57

SKU: 396
Details
Details
BA Slotted Cheese Head Machine Screw Grade-4.8 BS57
dd maxdk maxdk mink maxk minn maxn mint nom
0BA0.23600.41300.40300.16700.15900.06400.05600.0750
1BA0.20900.36600.35600.14800.14100.05800.05000.0660
2BA0.18500.31900.30900.13000.12300.05200.04400.0580
3BA0.16100.28300.27300.11300.10700.04700.03900.0510
4BA0.14200.25200.24200.10100.09500.04000.03400.0450
5BA0.12600.22100.21100.08800.08300.04000.03400.0400
6BA0.11000.19400.18400.07800.07300.03300.02700.0350
7BA0.09800.17300.16300.06900.06400.03300.02700.0310
8BA0.08700.15700.14700.06300.05900.03000.02400.0270
9BA0.07500.12800.12300.05200.04800.03000.02400.0240
10BA0.06700.11200.10700.04500.04100.02400.01900.0200
11BA0.05900.11000.10500.04500.04100.02400.01900.0200
12BA0.05100.09500.09000.03800.03500.02000.01500.0170
13BA0.04700.08100.07600.03200.02900.02000.01500.0140
14BA0.03900.06400.05900.02600.02300.01500.01100.0120
15BA0.03500.06400.05900.02600.02300.01500.01100.0120
16BA0.03100.05800.05400.02300.02000.01300.00900.0100
Additional Info
Additional Info
Weight0.0000
MaterialGrade-4.8
Standard NumberBS57
Second Standard-
DriveSlot
HeadCHEESE
American Generic Brand Term-
Diameter 0BA,1BA,2BA,3BA,4BA,5BA,6BA,7BA,8BA,9BA,10BA,11BA,12BA,13BA,14BA,15BA,16BA
Length1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2."