Inch Slotted Raised Countersunk Head Self Tapping Screw AB Case Hardened Steel BS4174
Loading...
Zoom

Inch Slotted Raised Countersunk Head Self Tapping Screw AB Case Hardened Steel BS4174

SKU: 488
Details
Details
Inch Slotted Raised Countersunk Head Self Tapping Screw AB Case Hardened Steel BS4174
ddk maxdk mink nomf nomn maxn mint nom
No.20.17200.14700.05100.02500.03100.02300.0410
No.40.22500.19500.06700.03300.03900.03100.0540
No.60.27900.24400.08300.04000.04800.03900.0670
No.80.33200.29200.10000.04800.05400.04500.0800
No.100.38500.34000.11600.05500.06000.05000.0940
No.120.43800.38900.13200.06300.06700.05600.1070
No.140.50700.45200.15300.07200.07500.06400.1240
No.160.63500.56800.19100.09000.08400.07200.1560