d e s max s min k max k min f Max f Min g Max g Min
1/4"0.51000.44500.43800.17600.16600.25000.24700.42800.4180
5/16"0.61000.52500.51800.21800.20800.31300.30900.50800.4980
3/8"0.69000.60000.59200.26000.25000.37500.37200.58200.5720
7/16"0.82000.71000.70200.30200.29200.43800.43400.69000.6800
1/2"0.95000.82000.81200.34300.33300.50000.49600.80000.7900
9/16"1.06000.92000.91200.37500.36500.56300.55900.90000.8900
5/8"1.17001.01001.00000.41700.40700.62500.61900.98500.9750
3/4"1.39001.20001.19000.50000.48000.75000.74401.17501.1650
7/8"1.50001.30001.28800.58300.56300.87500.86701.27301.2630
1"1.71001.48001.46800.66600.63601.00000.99201.45301.4330
1.1/8"1.93001.67001.64000.75000.71001.12501.11701.62001.6100
1.1/4"2.15001.86001.81500.83000.79001.25001.24201.79501.7850
1.3/8"2.37002.05002.00500.92000.88001.37501.36501.98501.9750
1.1/2"2.56002.22002.17501.00000.96001.50001.49002.15502.1450
1.3/4"2.98002.58002.52001.17001.11001.75001.74002.49502.4850
2"3.19002.76002.70001.33001.27002.00001.99002.67502.6650