G 1/8"3.000014.000011.00005.0000
G 1/4"3.000018.000015.00006.0000
G 3/8"3.000022.000015.00008.0000
G 1/2"4.000026.000018.000010.0000
G 3/4"4.000032.000020.000012.0000
G 1"5.000039.000021.000017.0000
G 1.1/8"5.000044.000021.000019.0000
G 1.1/4"5.000049.000021.000022.0000
G 1.1/2"5.000055.000021.000024.0000
G 1.3/4"5.000062.000025.000032.0000
G 2"5.000068.000025.000032.0000