Technical Information
Fastener Specific
Supply Source

NPTF 3/4 Taper Socket Taper Pressure Pipe Plugs Alloy Steel B1.20.3
Loading...
Zoom

NPTF 3/4 Taper Socket Taper Pressure Pipe Plugs Alloy Steel B1.20.3

SKU: 1892
Details
Details
NPTF 3/4 Taper Socket Taper Pressure Pipe Plugs Alloy Steel B1.20.3
Dtpidbb maxb minstg
1/16"270.3125/16"0.3240.35/32"0.140.062
1/8"270.4055/16"0.3240.33/16"0.140.062
1/4"180.547/16"0.4570.4171/4"0.2180.073
3/8"180.6751/2"0.520.485/16"0.250.084
1/2"140.849/16"0.5820.5423/8"0.3120.095
3/4"141.055/8"0.6450.6059/16"0.3120.125
1"375611.3153/4"0.770.735/8"0.3750.125
1-1/4"375611.6613/16"0.8320.7923/4"0.4370.156
1-1/2"375611.913/16"0.8430.781"0.4370.156
2"375612.3757/8"0.9060.8441"0.4370.156
Additional Info
Reviews
Tags