UNF Hexagon Full Nut Mild Steel A-A563 B18.2.2
DDss maxs mine maxe minmm maxm min
1/4"0.25007/16"0.43800.42800.50500.48807/32"0.22600.2120
5/16"0.31251/2"0.50000.48900.57700.557017/64"0.27300.2580
3/8"0.37509/16"0.56200.55100.65000.628021/64"0.33700.3200
7/16"0.437511/16"0.68800.67500.79400.76803/8"0.38500.3650
1/2"0.50003/4"0.75000.73600.86600.84007/16"0.44800.4270
9/16"0.56257/8"0.87500.86101.01000.982031/64"0.49600.4730
5/8"0.625015/16"0.93800.92201.08301.051035/64"0.55900.5350
3/4"0.75001-1/8"1.12501.08801.29901.240041/64"0.66500.6170
7/8"0.87501-5/16"1.31201.26901.51601.44703/4"0.77600.7240
1"1.00001-1/2"1.50001.45001.73201.653055/64"0.88700.8310
1-1/8"1.12501-11/16"1.68801.63101.94901.859031/32"0.99900.9390
1-1/4"1.25001-7/8"1.87501.81202.16502.06601-1/16"1.09401.0300
1-3/8"1.37502-1/16"2.06201.99402.38202.27301-11/64"1.20601.1380
1-1/2"1.50002-1/4"2.25002.17502.59802.48001-9/32"1.31701.2450