Inch Pipe Thread Pipe Nut Grade-14.9-45H DIN431
Dsem
G 1/8"19.000020.88006.0000
G 1/4"22.000023.91006.0000
G 3/8"27.000029.56007.0000
G 1/2"32.000035.03008.0000
G 5/8"32.000035.04008.0000
G 3/4"36.000039.55009.0000
G 7/8"41.000045.10009.0000
G 1"46.000050.850010.0000
G 1.1/8"50.000055.370010.0000
G 1.1/4"55.000060.790011.0000
G 1.1/2"60.000066.440012.0000
G 1.3/4"70.000076.930013.0000
G 2"75.000082.800013.0000
G 2.1/4"85.000093.500016.0000
G 2.1/2"96.0000105.600016.0000
G 3"105.0000115.500019.0000
G 4"135.0000148.500022.0000
G 5"165.0000181.500022.0000
G 6"190.0000209.000025.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-14.9-45H
Standard NumberDIN431
Second Standard-
DriveHexagon
HeadNON
American Generic Brand Term-
Diameter G1/8",G1/4",G3/8",G1/2",G5/8",G3/4",G7/8",G1",G1.1/8",G1.1/4",G1.1/2",G1.3/4",G2",G2.1/4",G2.1/2",G3",G4",G5",G6"