Metric Coarse Hexagon Spherical Face Nut Length 1.5D Class-10 DIN6330B

SKU: 703
Details
Details

Metric Coarse Hexagon Spherical Face Nut Length 1.5D Class-10 DIN6330B

 

dd1hrs
M8 9.00 12.00 11.00 13.00
M10 11.50 15.00 15.00 16.00
M12 14.00 18.00 17.00 18.00
M14 16.00 21.00 20.00 22.00
M16 18.00 24.00 22.00 24.00
M20 22.00 30.00 27.00 30.00
M24 26.00 36.00 32.00 36.00
M30 32.00 45.00 41.00 46.00
M36 38.00 54.00 50.00 55.00


Metric Coarse Hexagon Spherical Face Nut Length 1.5D Class-10 DIN6330B

Additional Info
Additional Info
Weight0.0000
MaterialClass-10
Standard NumberDIN6330B
Second Standard-
DriveHexagon
HeadNON
American Generic Brand TermHEXCONNECTORNUT
Diameter M6,M8,M10,M12,M16,M20,M24,M30,M36,M42,M48
LengthNON