BSF Hexagon Lock Nut Thicker 3 Sizes Grade-A-Steel BS1083
d | e | s max | s min | m max | m min |
---|---|---|---|---|---|
1/4" | 0.5100 | 0.4450 | 0.4380 | 0.1610 | 0.1510 |
5/16" | 0.6100 | 0.5250 | 0.5180 | 0.1930 | 0.1820 |
3/8" | 0.6900 | 0.6000 | 0.5920 | 0.2240 | 0.2140 |
Weight | 0.0000 |
---|---|
Material | Grade-A-Steel |
Standard Number | BS1083 |
Second Standard | - |
Drive | Hexagon |
Head | NON |
American Generic Brand Term | HALFNUT,JAMNUT |
Diameter | 1/4",5/16",3/8" |
Length | NON |